Jaguar
Physical, mechanical and technological specifications:
Hardness
(Mohs)
3-4
Unit Volume Weight
(gr/cm3)
2,67
Density
(gr/cm3)
2,74
Water absorption at atmospheric pressure
by weight (%)
0,10
 
by volume (%)
0,10
Water absorption at boiling water
by weight (%)
0,10
 
by volume (%)
0,10
Prosity
(%)
0,64
Compressive strength
(Kg/cm2)
914,48
Compressive strength after freesing
(Kg/cm2)
708,73
Strength to blow
(Kg/cm2)
8,39
Strength to bending
(Kg/cm2)
121,51
Modulus of Elasticity
(Kg/cm2)
9,94x10³
Ratio of fulllness
(%)
99,30
Degree of pores
(%)
0,82
Average Abrasion Loss
(cm3/50 cm2)
3,85
Average Tensile Strength
(Kg/cm2)
79,00
Chemical analysis:
CaO
 
43,20
MgO
 
9,20
SiO2
 
1,50
A12O3
 
-
Fe2O3
 
0,84
CaCO2
 
-
MgO3
 
-
K2O
 
-
TlO2
 
-
A.Z.
 
-
Others
 
-